20oC 60oC 100oC
Acetaldehyde ND ND ND
Acetic acid (10%) R R ND
Acetic acid (glac./anh.) ND ND ND
Acetic anhydride ND ND ND
Aceto-acetic ester ND ND ND
Acetone ND ND ND
Other ketones ND ND ND
Acetonitrile ND ND ND
Acetylene ND ND ND
Acetyl salicylic acid ND ND ND
Acid fumes ND ND ND
Alcohols ND ND ND
Aliphatic esters ND ND ND
Alkyl chlorides ND ND ND
Alum ND ND ND
Aluminium chloride ND ND ND
Aluminium sulphate ND ND ND
Ammonia, anhydrous ND ND ND
Ammonia, aqueous ND ND ND
Ammonium chloride ND ND ND
Amyl acetate ND ND ND
Aniline ND ND ND
Antimony trichloride ND ND ND
Aqua regia ND ND ND
Aromatic solvents ND ND ND
Ascorbic acid ND ND ND
Beer ND ND ND
Benzaldehyde ND ND ND
Benzene ND ND ND
Benzoic acid ND ND ND
Benzoyl peroxide ND ND ND
Boric acid ND ND ND
Brines, saturated ND ND ND
Bromide (K) solution ND ND ND
Bromine ND ND ND
Bromine liquid, tech. ND ND ND
Bromine water, saturated aqueous ND ND ND
Butyl acetate ND ND ND
Calcium chloride ND ND ND
Carbon disulphide ND ND ND
Carbonic acid ND ND ND
Carbon tetrachloride ND ND ND
Caustic soda & potash ND ND ND
Cellulose paint ND ND ND
Chlorates of Na, K, Ba ND ND ND
Chlorine, dry ND ND ND
Chlorine, wet ND ND ND
Chlorides of Na, K, Ba ND ND ND
Chloroacetic acid ND ND ND
Chlorobenzene ND ND ND
Chloroform ND ND ND
Chlorosulphonic acid ND ND ND
Chromic acid (80%) ND ND ND
Citric acid ND ND ND
Copper salts (most) ND ND ND
Cresylic acids (50%) ND ND ND
Cyclohexane ND ND ND
Detergents, synthetic ND ND ND
Emulsifiers, concentrated ND ND ND
Esters ND ND ND
Ether ND ND ND
Fatty acids (>C6) ND ND ND
Ferric chloride ND ND ND
Ferrous sulphate ND ND ND
Fluorinated refrigerants ND ND ND
Fluorine, dry ND ND ND
Flourine, wet ND ND ND
Fluorosilic acid ND ND ND
Formaldehyde (40%) ND ND ND
Formic acid ND ND ND
Fruit juices ND ND ND
Gelatine ND ND ND
Glycerine ND ND ND
Glycols ND ND ND
Glycol, ethylene ND ND ND
Glycolic acid ND ND ND
Hexamethylene diamine ND ND ND
Hexamine ND ND ND
Hydrazine ND ND ND
Hydrobromic acid (50%) ND ND ND
Hydrochloric acid (10%) ND ND ND
Hydrochloric acid (conc.) ND ND ND
Hydrocyanic acid ND ND ND
Hydrofluoric acid (40%) ND ND ND
Hydrofluoric acid (75%) ND ND ND
Hydrogen peroxide (30%) ND ND ND
Hydrogen peroxide (30 - 90%) ND ND ND
Hydrogen sulphide ND ND ND
Hypochlorites ND ND ND
Hypochlorites (Na 12-14%) ND ND ND
Iso-butyl-acetate ND ND ND
Lactic acid (90%) ND ND ND
Lead acetate ND ND ND
Lead perchlorate ND ND ND
Lime (CaO) ND ND ND
Maleic acid ND ND ND
Manganate, potassium (K) ND ND ND
Meat juices ND ND ND
Mercuric chloride ND ND ND
Mercury ND ND ND
Methanol ND ND ND
Methylene chloride ND ND ND
Milk products ND ND ND
Moist air ND ND ND
Molasses ND ND ND
Monoethanolamine ND ND ND
Naptha ND ND ND
Napthalene ND ND ND
Nickel salts ND ND ND
Nitrates of Na, K and NH3 ND ND ND
Nitric acid (<25%) ND ND ND
Nitric acid (50%) ND ND ND
Nitric acid (90%) ND ND ND
Nitric acid (fuming) ND ND ND
Nitrite (Na) ND ND ND
Nitrobenzene ND ND ND
Oils, diesel ND ND ND
Oils, essential ND ND ND
Oils, lubricating + aromatic additives ND ND ND
Oils, mineral ND ND ND
Oils, vegetable and animal ND ND ND
Oxalic acid ND ND ND
Ozone ND ND ND
Paraffin wax ND ND ND
Perchloric acid ND ND ND
Petroleum spirits ND ND ND
Phenol ND ND ND
Phosphoric acid (20%) R R ND
Phosphoric acid (50%) R R ND
Phosphoric acid (95%) ND ND ND
Phosphorous chlorides ND ND ND
Phosphorous pentoxide ND ND ND
Phthalic acid ND ND ND
Picric acid ND ND ND
Pyridine ND ND ND
Salicyl aldehyde ND ND ND
Sea water ND ND ND
Silicic acid ND ND ND
Silicone fluids ND ND ND
Silver nitrate ND ND ND
Sodium carbonate ND ND ND
Sodium peroxide ND ND ND
Sodium silicate ND ND ND
Sodium sulphide ND ND ND
Stannic chloride ND ND ND
Starch ND ND ND
Sugar, syrups & jams ND ND ND
Sulphamic acid ND ND ND
Sulphates (Na, K, Mg, Ca) ND ND ND
Sulphites ND ND ND
Sulphonic acids ND ND ND
Sulphur ND ND ND
Sulphur dioxide, dry ND ND ND
Sulphur dioxide, wet ND ND ND
Sulphur dioxide (96%) ND ND ND
Sulphur trioxide ND ND ND
Sulphuric acid (<50%) ND ND ND
Sulphuric acid (70%) ND ND ND
Sulphuric acid (95%) ND ND ND
Sulphuric acid, fuming ND ND ND
Sulphur chlorides ND ND ND
Tallow ND ND ND
Tannic acid (10%) ND ND ND
Tartaric acid ND ND ND
Trichlorethylene ND ND ND
Urea (30%) ND ND ND
Vinegar ND ND ND
Water, distilled. ND ND ND
Water, soft ND ND ND
Water, hard ND ND ND
Wetting agents (<5%) ND ND ND
Yeast ND ND ND
Zinc chloride ND ND ND

 